chemical composition:
cu ≥98.5%
cr:0.5-1.5%
zr:0.08-0.30%
mechanical properties:
tensile strength:≥400mpa
yeild strength:≥280mpa
hardness: ≥100
elongation:≥15%
conductivity:≥80%iacs
softening temperature:≥500°c
|